NANOCLEAN-50 is a desizing & scouring agent
for heavily sized polyester their blends. It reduces cost per batch.
Except caustic soda you will not add other pretreatment auxiliaries like
stain remover,soda ash, desizing chemicals, soap etc.
FEATURES:
- Environmental Friendly, Oil Removing and Scouring Agent
- Highly
efficient scouring and multifunctional dyeing agent.
- A
multi functional product which provides bleaching and brightening effects.
- Along
with cleaning it also makes fabric soft.
- Get
150% to 200% production in same expenses.
- It
removes texturing and weaving oil and size
- Reduces
quantity of caustic & hydro required for processing synthetic fabrics.
- Acts
as a dye career and leveling agent
- Compared
with traditional process, less damage to fabric and enhanced economic efficacy.
- Effective
cleaning, less water and energy consumption
- No
need to add emulsifier or N.I.D as it is mixed in the formulation.
PROPERTIES
- COMPOSITION : Blend of non-ionic surfactants and
specialty chemicals
- APPEARANCE : colorless to pale yellow liquid
- SOLUBILTY : Easily miscible with water
APPLICATIONS
OF NANOCLEAN-50:
PROCESS FOR SCOURING 100% POLYESTER
CLOTH PROCESS: Take 100 kgs of polyester cloth. At 60 °C add 1 KG of NANOCLEAN-50 & add acetic acid to maintain PH-4
& then add required amount of color. Raise the temperature up to 120 °C to 130 °C in jet dyeing. Holding time is 30
minutes per batch.
ADVANTAGE: NANOCLEAN-50 saves water, power, fuel & labour
cost.
(2) Weight Reduction process:
(A) Use 1 KG NANOCLEAN-50, with caustic soda
in 100 kgs cloth
Advantage: it gives better swelling, wetting and
gives even weight reduction.
(b) After weight reduction as per above
standard process repeat the application (1)
ADVANTAGE: It gives even weight reduction, removes spinning oil, size & other
impurities. Cloth gets excellent brightness, extra bouncing effect & 10 to
15 % enhanced color depth.
(3)
Drum process:
Addition of 1 KG. Of NANOCLEAN-50 , in 100 kgs, Cloth in usual process.
Advantage: It saves time. Process is possible
even at lower temperature. It gives better swelling, extra bounce, relaxation
of yarn and better disability.
POLYESTER
BLENDED CLOTH PROCESS
TOP DYED (YARN DYED) FABRIC PROCESS :
Take 100 kgs,of polyester viscose cloth
in jet dyeing machine. Add 1.5 KG NANOCLEAN-50 and & add acetic acid to maintain
PH-4 and required amount of WHITE-R & RANIPAL. Raise the temperature up to
80 °C to 90 °C in jet scouring. Holding time required is only 30 minutes per batch. In Jigger
dyeing raise the temperature upto 80 °C to 90 °C.
Double
dyeing process:Take 100 kgs of polyester viscose clothe. At 60 °C add 1 KG NANOCLEAN-50 with disperse
& reactive colour. Now add acetic acid to maintain PH-4 and 10 kgs common
salt. Raise the temperature up to 130 °C. Hold for 10 minutes. Add 2 kgs soda
ash & again hold for 10 minutes. Now drain the bath and give plain wash
with acetic acid.
|